"G-40 equivalent" / "G40e"

Has anyone encountered this?
http://tinyurl.com/mwvvx2a

Obviously, Marino-Ware has “a dog in [this] fight”, but this is something for which I’ll nonetheless be on the lookout…

I just received the flyer from M-W. Pretty sad if this is happening. I haven’t heard of it but I guess we need to put our CA folks on alert.

G40e? How sad is this?

Regardless of M-W’s involvement, it sounds like another attempt to slip an inferior product by us diligent spec writers! I have alerted our people in our CA offices, and some friends in other firms to “be on the look out” for this stuff.

How many LEED accredited youngsters just starting in CA will automatically assume that the “e” in G40e means this must be the better product because it must be good for the environment?

Perhaps Diet G-40 is more accurate.

I agree with the above on notifying CA, but I also revised our office spec section.

I am just surprised that I have not heard anything from Clark Dietrich or other major steel stud manufacturers.

Clark Dietrich, as well as most other manufactures of steel framing, offers all three types of coatings: hot-dipd glavanized (G40, G60), and equivalent coatings G40E and CP60, for example. If you want galvanized coatings, simply specify the coating to be “ASTM A653/A653M, G40, hot-dip galvanized.”

What’s the big deal about this anyway? If the protective coating does what it is supposed to do (protect the steel from corrosion while exposed on the job site, prior to the building being dried-in), what difference does is make whether it’s zinc or something else?

I believe anon may bring up a valid point (even if his point was made jokingly. can not gauge sarcasm online). There are a lot of various steel stud installation details and locations within a typical structure (office building for instance). We would routinely specify different gauges, etc. for the various areas. The studs at the curtain wall are often different than the interior studs separating two typical offices. Is it possible that you could utilize “Diet G-40” for some of the studs that are less likely to be exposed to potential fenestration leaks, condensation issues, etc.

My gut reaction is to use G40,hot dip for everything and specifically exclude G40e as an option but maybe it does have it’s place as long as it’s place is clearly defined.

I think the original purpose of this thread has gotten lost in the shuffle. The issue wasn’t over G60 or G40. It was the fact that the steel stud material was coming from China, and that the referenced G40e was not even an ASTM Standard coating system.

Also, Ken’s CA reference wasn’t to Contruction Administration but to our California office.

Conspectus has a good info page about standard zinc coatings - http://www.conspectusinc.com/downloads/Documents/Conspectus%20Tech%20Tips%20C1010%20Zinc%20Coatings%20and%20Metal%20Studs%20rev10.12.30.pdf.

To anon: Why should my client pay the same amount for an unknown quantity (G40e) instead of a known level of protection (G40). G40 has been an industry standard for interior framing for years. Keep in mind that framing does not appear miraculously on-site, transported to a nice, dry environment. It tends to sit around bundled up outside getting damp or wet. I know what to expect from a G40 coating that meets ASTM standards. I have no idea what to expect from a coating that is being passed off as something ‘just as good as G40’. Once there is an equivalent ASTM standard for G40e, I’ll take a look at it. Right now, it has taken up way more of my time than I’m comfortable with.

To Ken: Your client wouldn’t be paying for G40 in getting G40e, your client would be paying less for G40e which would in all likelihood be a perfectly acceptable level of protection for 99% of all the steel studs in the building. And maybe the reputation of our profession would be helped just a little bit in recognizing that it’s not always about “i’ve done it this way for 30 years, blah, blah, blah…” in today’s world, and more about providing good service to our clients.

Do you really think that a little bit of oxidation on steel studs installed in the interior of a building is some sort of major issue? It is not. Have you considered that maybe, just maybe, we have been over-specifying when requiring G40 protection and that clients have been needlessly spending more money for this?

I see rust on interior structural steel members on job sites all the time. No prob. There is no requirement for primer on structural steel. I specify screws with either galvanized coatings or proprietary corrosion resistant coatings all the time. Never had a problem with the coatings.

Again, I ask, what is the big deal?

Sounds like you have a dog in this fight. My dog is to protect my clients and, again, I’m going to stay with what I know until I know what the other option actually provides. If this option is so good, why isn’t there an industry standard for it? I’m usually among the first to try new technologies. I just like to know what I’m using before I buy into it.

I’m an open book in what I say and what I do. Why stay anonymous? Who do you work for?

Why does it matter who I work for? My points are just as valid as anyone else that is allowed to post (thank you, Colin) on this forum.

I don’t have a dog in this fight. I am learning about this for this first time. I am a specifier for a large firm. I did a little more research and found out that BEFORE galvanized coatings on steel studs were standard, red oxide paint was used - on cold formed steel studs. Paint. No issues with corrosion protection. Ever. The reason paint went away was due to more and more restrictions on VOCs. Enter galvanizing.

The ASTM standards that govern protective coatings on steel studs allow multiple types of coatings. Not limited to only G40 or G60 zinc. The standards allow G40e as long as it meets the minimum performance established in the standard. One manufacturer I spoke with that provides this type of coating, Clark Dietrich, has lab testing showing their G40e coating far outperforms a G40 coating when subjected to salt spray. It’s better than G40.

The G40e coating from Clark Dietrich is actually TWO coatings - a proprietary coating OVER a galvanized coating - the latter deposited over the base metal at the mill.

In some cases the G40e is less costly than G40 - so not only will you get better corrosion resistance, but at a cheaper price.

I think my clients will appreciate that I know what I am talking about when it comes to this, and that I am not blindly going along with the manufacturer that doesn’t like (because it cannot provide) a superior, less costly G40e coating. I also think that my clients will appreciate that I am not stubbornly adherent to some antiquated way of doing something just because it’s always been done that way. In this case, that would mean sticking with red oxide paint over plain steel studs.

@anon: I think you are missing Ken’s point here. He is fine with the other material if it has a test. We can let you be the first to test it out without the ASTM. You might want to talk with your insurance carrier before proceeding as you might be paying for it out of your pocket. You may also need to review all the codes to be sure that you are not in violation of building codes. I remember when certain Chinese bolts began to fail because they did not meet US specifications. As far as your comment about the 30 years experience, well as any risk taker will discover, when you fail, it will cost you. Those tests and standards are there for a reason, HSW. All you imply that you want to do is provide your client an untested method that saves him some initial cost. The cost of replacement later may be a lot more than he expected, since he did not expect to have it fail in the first place. You also state that you feel that “just maybe, we have been over-specifying when requiring G40 protection…” Interesting statement when mold and mildrew is one large problem in the construction industry today. That means that water is present. That is why the specifications usually require this. That was the 30 years experience that has shown it.

Finally, check out the case in court with the shopping mall in Canada. The collapse killed people. The roof leaked and the structure rusted. The client tried a coating that never worked from day one. The architect was dragged into the case 25 years after the fact. The cost of that defense and the lawyers he had to get costs money. That is why these tests exist and why we always want to be safe about it. HSW is where the buck stops.

Anon: A little surface rust on rolled structural steel members is much different than rust on sheet steel studs, which are a fraction of the thickness of rolled members.

Anon: I tend to stay out of dog fights since they usually solve nothing and take time away from other things I want to do. That said, in your post of August 06, 2013 - 06:22 pm made some statements that are incorrect

No issues with corrosion protection. Ever..  I have vivid memories of badly rusted painted studs on several projects I have worked on since I started in 74.  Corrosion was definitely an issue. 
The reason paint went away was due to more and more restrictions on VOCs. While VOCs might have been an issue, the fact that galvanization works even if the coating is scratched was (and is) more of an issue.  Even screws in painted studs create potential corrosion sites much more readily than screws in galvanized studs.

Clark Dietrich has been a player for a long time and knows the drill. If this new coating is, in fact, as good or better than G40, that’s great. They’re a big enough player and are involved in ASTM. If they want to change the industry, it’s incumbent on them to prove their case. That means giving the industry a standard that we can use. I’m not going to give them a competitive advantage just because they say so. I’m not from Missouri, but they still need to show me.

It sounds like you’ve researched this a lot more than I have. Is this coating self-healing like other zinc coatings? Again, you might not care about rusted studs, but as others have already noted, fastener failures and other problems are just that, problems. Why should I make my life more difficult, and increase my potential liability, on the promise to save my clients a small fraction of a percent of the cost of the project which they may or may not see?

My comments were specific to what this thread is about - INTERIOR non-structural metal stud framing, and all of my comments are accurate; no corrosion issues, no rusted/failed screws, etc.

I have not addressed EXTERIOR enclosure cold-formed load-bearing metal stud framing. That is a different topic, with a different set of issues. I would not specify G40 or G40e for exterior enclosure cold-formed metal framing - my minimum for this is CP60 - which is in the standard.

I say again - G40e is addressed in the ASTM standards. Clark Dietrich has nothing to prove, they comply with the specified standards. it is Marino/Ware that is unnecessarily stirring the pot on this, in my opinion, because they can’t compete. I am sure that they had their say in the Standards development as well, and that any objections they raised were ultimately dismissed by the committee members. That’s how the consensus process works.

The advice to specifiers from Marino/Ware to exclude any and all Standard-acceptable coatings except galvanized will most certainly cause you trouble at some point, because you will have to come up with some sort of justification why. There is none.

I wanted to weigh in on this issue. I am the Code Development Manager for ClarkDietrich, a Fellow of ASTM, and I am currently the Chairman of ASTM Committee C11 (which has jurisdiction over ASTM C645) and Vice Chairman of Committee A05 (which has jurisdiction over A1003, which covers the metallic coated sheet steel specified in C645).

I think it is important to separate the facts from the innuendo. The issue of whether EQ coating are permissible is a veiled attempt by some to confuse specifiers and users into believing that only one particular coating type meets the specification requirements. Lets look at what the code requires and then you decide.

The IBC specifies in Chapter 25, Table 2506.2, that nonstructural studs should meet the requirements of ASTM C645. This is the code requirement that all manufacturers must conform to. This has been the code requirement since the I-codes were written and possibly before then. ASTM C645, paragraph 4.2 has specific requirements for the coating used on the studs. It specifically states Members shall have a protective coating conforming to Specification A653/A653M G 40 minimum or shall have a protective coating with an equivalent corrosion resistance.

How do we know the coatings provide equivalent corrosion resistance? The coatings used are typically tested side-by-side against a known sample of G40, using the ASTM B117 testing procedure. Test results prove that equivalent coatings outlast the corrosion protection of the G40 coating.

The SFIA, the largest steel stud industry association, representing the vast majority of all of the tonnage used in the manufacture of cold-formed steel framing with an all-inclusive membership of manufacturers, distributors, contractors, and engineers, in its Code Compliance Certification Program recognizes EQ coatings and has incorporated them into their compliance program. Manufacturer members of the SFIA using EQ coatings are subject to random unannounced inspections and have products chosen and tested using the B117 procedure to make sure they meet the program requirements.

SFIAs Code Compliance Certification Program IS THE ONLY ONE ENDORSED BY THE ASSOCIATION OF WALLS AND CEILINGS (AWCI).

Our EQ coated products meet or exceed the minimum IBC Code standards as set forth by ASTM specifications and the Code Compliance Certification Program of the SFIA. We have hundreds of thousands of hours of testing to prove the coatings meet the requirements and we are third party audited, tested, and certified.

ANON is correct in his posted statements. If you take the time to look at the requirements you will see that your clients are not getting less and paying more. They are in fact getting a Code Compliant coating that is superior to a G40 coating.

Thanks Michael. Looking at C645 I don’t see a G40e designation. Please explain where the performance criteria for that is located.